HAUTE BRIQUE D'ALUMINE
ARTICLES | INDEX | ||||||
LZ-75 | LZ-65 | LZ-55 | LZ-48 | ||||
% du ≥ Al2O3 | 75 | 65 | 55 | 48 | |||
CARACTÈRE RÉFRACTAIRE ≥ OC | 1790 | 1790 | 1770 | 1750 | |||
COMMENCEZ LA TEMPÉRATURE de RAMOLLISSEMENT SOUS % de ≥ de la CHARGE 0.2MPA | 1520 | 1500 | 1470 | 1420 | |||
CHANGEMENT % DE REVÊTEMENT DE REFIRIRNG | 1500 OC, 2h | +0.1 -0.4 | |||||
1450 OC, 2h | +0.1 -0.4 | ||||||
% DE ≤ DE POROSITÉ APPARENTE | 23 | 22 | |||||
FORCE Mpa≥ de BROYAGE À FROID | 53.9 | 49.0 | 44.1 | 39.2 | |||
China